Complementary analyses of aging in a commercial LiFePO4/graphite 26650 cell
Tech Univ Denmark, Dept Energy Convers & Storage, DTU Energy, Frederiksborgvej 399, DK-4000 Roskilde, Denmark;Northwestern Univ, Dept Mat Sci & Engn, 2220 Campus Dr, Evanston, IL 60208 USA.
Tech Univ Denmark, Dept Energy Convers & Storage, DTU Energy, Frederiksborgvej 399, DK-4000 Roskilde, Denmark.
Aalborg Univ, Dept Energy Technol, Fredrik Bajers Vej 5, DK-9100 Aalborg, Denmark.
Uppsala University, Disciplinary Domain of Science and Technology, Chemistry, Department of Chemistry - Ångström, Structural Chemistry.ORCID iD: 0000-0003-2538-8104
Show others and affiliations
2018 (English)In: Electrochimica Acta, ISSN 0013-4686, E-ISSN 1873-3859, Vol. 284, p. 454-468Article in journal (Refereed) Published
Abstract [en]

In this work we investigate the electrode degradation mechanisms in a commercial 2.5 Ah LiFePO4/ graphite 26650 cylindrical cell. Aged and fresh electrode samples were prepared by cycling two cells respectively five and 22 k times. Subsequently the cells were disassembled in a glovebox and the electrode samples were prepared for electrochemical testing in a 3-electrode setup, and for characterization with XRD, XPS and low-kV FIB/SEM tomography. A 1 mu m thick CEI (cathode electrolyte interface) layer was observed at the electrode/electrolyte interface of the aged LiFePO4 electrode. Relative to the fresh LiFePO4 electrode, the aged electrode exhibited a larger series resistance which indicates the observed degradation layer increases the ionic resistance. In addition, micron-sized agglomerates, probably a mixture of carbonaceous material and decomposition products from the electrolyte, were observed at the electrode/electrolyte interface of the aged graphite electrode. These layers may contribute significantly to the loss of lithium inventory (LLI) in the cell, and to the loss of active material (LAM) in the graphite electrode. Low-voltage FIB/SEM tomography was used to detect local charging effects of graphite particles in the carbon electrode, an effect of poor dissipation of the electric charge to the ground after the sample interaction with the electron beam. The charging effects were primarily observed in the aged electrode and most of the locally charged particles were found to be close to the electrode/electrolyte interface, indicating a poorly percolating graphite network near this interface.

Place, publisher, year, edition, pages
2018. Vol. 284, p. 454-468
Keywords [en]
Li-ion battery, Cathode electrolyte interface, Electrochemical impedance spectroscopy, Degradation mechanisms, Focused ion beam
National Category
Materials Chemistry
Identifiers
URN: urn:nbn:se:uu:diva-366152DOI: 10.1016/j.electacta.2018.07.124ISI: 000442485100051OAI: oai:DiVA.org:uu-366152DiVA, id: diva2:1264339
Available from: 2018-11-20 Created: 2018-11-20 Last updated: 2018-11-20Bibliographically approved

Open Access in DiVA

No full text in DiVA

Other links

Publisher's full text

Authority records

Younesi, Reza

Search in DiVA

By author/editor
Younesi, RezaHjelm, Johan
By organisation
Structural Chemistry
In the same journal
Electrochimica Acta
Materials Chemistry

Search outside of DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetric score

doi
urn-nbn
Total: 123 hits
CiteExportLink to record
Permanent link

Direct link
Cite
Citation style
  • apa
  • ieee
  • modern-language-association
  • vancouver
  • Other style
More styles
Language
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Other locale
More languages
Output format
  • html
  • text
  • asciidoc
  • rtf